AI 导读

Manipal College of Dental Sciences的体外研究表明,1.0%氧化镁纳米颗粒可显著降低自固化PMMA临时冠表面粗糙度(p=0.008),其弯曲强度(ISO 4049标准)在0.5%和1.0%浓度组均高于0.3%组(p<0.001),但与对照组无显著差异。

正文

Scientific Reports (2026) Cite this article

We’re sharing this article early to provide faster access to peer-reviewed, accepted research. It is citable and carries a permanent DOI. This version is subject to further edits and will be replaced automatically by the final Version of Record. All legal disclaimers apply.

Abstract

This in vitro study evaluated the effects of magnesium oxide (MgO) nanoparticles on the flexural strength, surface roughness, and color characteristics of a self-cure polymethyl methacrylate (PMMA) provisional crown material. A commercially available PMMA resin was modified with 0.3, 0.5, or 1.0% w/w MgO nanoparticles, while unmodified resin served as the control. A total of 144 specimens were prepared and allocated equally among the four groups for the three outcome assessments. Surface roughness was measured using a contact profilometer, flexural strength was determined using a three-point bending test according to ISO 4049, and color coordinates were recorded using a spectrophotometer in the CIE L*a*b* system. Data were analyzed using the Kruskal–Wallis test followed by Dunn’s post-hoc test with Holm correction. Surface roughness differed significantly among the groups (p = 0.008), with the 1.0% MgO group exhibiting significantly lower roughness than the control. Flexural strength also differed significantly (p < 0.001); the 0.5 and 1.0% MgO groups showed significantly higher values than the 0.3% group, while none differed significantly from the control. L* and b* did not differ significantly among the groups, whereas a* showed a significant shift (p < 0.001). Control-referenced ΔE*ab values derived from the group mean CIELAB coordinates remained below established perceptibility and acceptability thresholds. Within the limitations of this study, 1.0% MgO reduced surface roughness while maintaining flexural strength and overall color characteristics comparable to the control.

Author information

Authors and Affiliations

  1. Department of Prosthodontics and Crown & Bridge, Manipal College of Dental Sciences Mangalore, Manipal Academy of Higher Education, Manipal, India

    Preetham Kotian

  2. Department of Prosthodontics and Crown & Bridge, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Manipal, India

    I. N. Aparna, Gayathri Krishnamoorthy, Gauri Shahi & Shilpa S. Prabhu

  3. Department of Public Health Dentistry, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Manipal, India

    Prajna Pramod Nayak

Authors

  1. Preetham Kotian
  2. I. N. Aparna
  3. Gayathri Krishnamoorthy
  4. Gauri Shahi
  5. Shilpa S. Prabhu
  6. Prajna Pramod Nayak

Corresponding authors

Correspondence to I. N. Aparna or Gauri Shahi.

Ethics declarations

Competing interests

The authors declare no competing interests.

Institutional review board statement

This in-vitro study did not involve human participants or any identifiable human data; therefore, informed consent was not applicable. The study was conducted in accordance with the ethical principles of the Declaration of Helsinki and the ethical approval to conduct the experimental procedures was obtained from the Institutional Ethics Committee; IEC2: 320/2023 (Kasturba Medical College and Kasturba Hospital, Manipal).

Additional information

Publisher’s note

Springer Nature remains neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Rights and permissions

Open Access This article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons licence, and indicate if changes were made. The images or other third party material in this article are included in the article’s Creative Commons licence, unless indicated otherwise in a credit line to the material. If material is not included in the article’s Creative Commons licence and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this licence, visit http://creativecommons.org/licenses/by/4.0/.

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Kotian, P., Aparna, I.N., Krishnamoorthy, G. et al. Effect of magnesium oxide nanoparticles on the flexural strength, surface roughness, and color of self-cure PMMA provisional crowns. Sci Rep (2026). https://doi.org/10.1038/s41598-026-74371-0